ASTM A744 / A744M - 10e1 standard specification for castings, iron-chromium-nickel, corrosion resistant, for severe service

0

Source: ASTM International

This specification covers standard requirements for iron-chromium-nickel alloy, stainless steel castings intended for particularly severe corrosive applications. Alloys shall be melted by the electric furnace process with or without refining such as argon-oxygen-decarburization. Castings shall be heat treated and shall conform to the required heat treatment conditions. The materials shall conform with the prescribed chemical requirements for carbon, manganese, silicon, phosphorus, sulfur, chromium, nickel, molybdenum, columbium, copper, selenium, tungsten, vanadium, iron, and nitrogen.

This abstract is a brief summary of the referenced standard. It is informational only and not an official part of the standard; the full text of the standard itself must be referred to for its use and application. ASTM does not give any warranty express or implied or make any representation that the contents of this abstract are accurate, complete or up to date.

1. Scope

1.1 This specification covers iron-chromium-nickel alloy, stainless steel castings intended for particularly severe corrosive applications.

1.2 This specification requires postweld heat-treatment of all weld repairs affecting surfaces intended to be wetted by the corrosive medium. For applications for which postweld heat-treatment is not considered mandatory for retention of acceptable corrosion resistance, refer to Specification A743/A743M.

Note 1—For general corrosion-resistant alloy castings, reference should be made to Specification A743/A743M. For general heat-resistant alloy castings, reference should be made to Specification A297/A297M. For nickel-base alloy castings, refer to Specification A494/A494M.

1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

1.3.1 Within the text, the SI units are shown in brackets.

1.3.2 Inch-pound units are applicable for material ordered to Specification A744 and SI units for material ordered to Specification A744M.

2. Referenced Documents (purchase separately)

ASTM Standards
A262 Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels
A297/A297M Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant, for General Application
A370 Test Methods and Definitions for Mechanical Testing of Steel Products
A494/A494M Specification for Castings, Nickel and Nickel Alloy
A732/A732M Specification for Castings, Investment, Carbon and Low Alloy Steel for General Application, and Cobalt Alloy for High Strength at Elevated Temperatures
A743/A743M Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
A781/A781M Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use
A957 Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use
E29 Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications

American Welding Society Standards
AWSA5.14 Specification for Nickel and Nickel Alloy Bare Welding Rods and Electrodes

Index Terms

austenitic stainless steel; corrosion; stainless steel; steel castings; Class codes (for metals/alloys); Corrosive service applications--castings; Iron-chromium castings--specifications ;

ICS Code

ICS Number Code 77.140.80 (Iron and steel castings)

DOI: 10.1520/A0744_A0744M-10E01

ASTM International is a member of CrossRef.

Customer comments

No comments were found for ASTM A744 / A744M - 10e1 standard specification for castings, iron-chromium-nickel, corrosion resistant, for severe service. Be the first to comment!